{"_buckets": {"deposit": "c0a363e5-1994-4bf7-a745-7e439caed3d5"}, "_deposit": {"created_by": 4, "id": "726", "owners": [4], "pid": {"revision_id": 0, "type": "depid", "value": "726"}, "status": "published"}, "_oai": {"id": "oai:niit.repo.nii.ac.jp:00000726", "sets": ["34"]}, "author_link": ["3827", "3828", "3825", "3826"], "item_6_biblio_info_6": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2010-07", "bibliographicIssueDateType": "Issued"}, "bibliographicPageEnd": "2", "bibliographicPageStart": "1", "bibliographicVolumeNumber": "53", "bibliographic_titles": [{"bibliographic_title": "日本建築学会北陸支部研究報告集"}]}]}, "item_6_description_14": {"attribute_name": "フォーマット", "attribute_value_mlt": [{"subitem_description": "application/pdf", "subitem_description_type": "Other"}]}, "item_6_description_39": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"subitem_description": "論文(Article)", "subitem_description_type": "Other"}]}, "item_6_description_4": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "コンクリートの表層面は意匠上かつ耐久性状上、重要な部位であることに着目し、その劣化現象を解明する上での基礎的実験を行った。その結果、水セメント比が等しく同一強度のコンクリートでも、単位水量(スランプ)が相違すれば、セメントペースト量や骨材量も異なることになり、表層モルタルの吸水性状が相違することを実験的に明らかにし、これより耐久性に及ぼす表層特性を考察した。", "subitem_description_type": "Abstract"}]}, "item_6_full_name_3": {"attribute_name": "著者別名", "attribute_value_mlt": [{"nameIdentifiers": [{"nameIdentifier": "3827", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Sato, Shigeharu"}]}, {"nameIdentifiers": [{"nameIdentifier": "3828", "nameIdentifierScheme": "WEKO"}], "names": [{"name": "Chino, Shigeo"}]}]}, "item_6_publisher_32": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "日本建築学会"}]}, "item_6_relation_41": {"attribute_name": "関係URI", "attribute_value_mlt": [{"subitem_relation_name": [{"subitem_relation_name_text": "http://ci.nii.ac.jp/naid/110008014695"}]}]}, "item_6_rights_12": {"attribute_name": "権利", "attribute_value_mlt": [{"subitem_rights": "社団法人日本建築学会"}, {"subitem_rights": "本文データは学協会の許諾に基づきCiNiiから複製したものである"}]}, "item_6_source_id_7": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0385-9622", "subitem_source_identifier_type": "ISSN"}]}, "item_6_source_id_9": {"attribute_name": "書誌レコードID", "attribute_value_mlt": [{"subitem_source_identifier": "AN00188761", "subitem_source_identifier_type": "NCID"}]}, "item_6_text_60": {"attribute_name": "URI", "attribute_value_mlt": [{"subitem_text_value": "http://hdl.handle.net/10623/31687"}]}, "item_6_version_type_15": {"attribute_name": "著者版フラグ", "attribute_value_mlt": [{"subitem_version_resource": "http://purl.org/coar/version/c_970fb48d4fbd8a85", "subitem_version_type": "VoR"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "佐藤, 茂治"}], "nameIdentifiers": [{"nameIdentifier": "3825", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "地濃, 茂雄"}], "nameIdentifiers": [{"nameIdentifier": "3826", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2020-02-25"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "110008014695.pdf", "filesize": [{"value": "238.7 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_note", "mimetype": "application/pdf", "size": 238700.0, "url": {"label": "110008014695.pdf", "url": "https://niit.repo.nii.ac.jp/record/726/files/110008014695.pdf"}, "version_id": "777cb208-a057-4ea3-b078-d9aace9a061e"}]}, "item_keyword": {"attribute_name": "キーワード", "attribute_value_mlt": [{"subitem_subject": "コンクリート表層", "subitem_subject_scheme": "Other"}, {"subitem_subject": "吸水性", "subitem_subject_scheme": "Other"}, {"subitem_subject": "コンクリートの単位水量", "subitem_subject_scheme": "Other"}, {"subitem_subject": "concrete surface", "subitem_subject_scheme": "Other"}, {"subitem_subject": "water absorption", "subitem_subject_scheme": "Other"}, {"subitem_subject": "water content per unit volume of concrete", "subitem_subject_scheme": "Other"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "conference paper", "resourceuri": "http://purl.org/coar/resource_type/c_5794"}]}, "item_title": "1-2 コンクリートの表層特性に関する実験研究(材料・構造系)", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "1-2 コンクリートの表層特性に関する実験研究(材料・構造系)", "subitem_title_language": "ja"}, {"subitem_title": "1-2 Experimental study on property of concrete surface", "subitem_title_language": "en"}]}, "item_type_id": "6", "owner": "4", "path": ["34"], "permalink_uri": "https://niit.repo.nii.ac.jp/records/726", "pubdate": {"attribute_name": "PubDate", "attribute_value": "2012-03-28"}, "publish_date": "2012-03-28", "publish_status": "0", "recid": "726", "relation": {}, "relation_version_is_last": true, "title": ["1-2 コンクリートの表層特性に関する実験研究(材料・構造系)"], "weko_shared_id": -1}
1-2 コンクリートの表層特性に関する実験研究(材料・構造系)
https://niit.repo.nii.ac.jp/records/726
https://niit.repo.nii.ac.jp/records/72667895627-2a7c-4ce2-ab11-fe2fc2979def
名前 / ファイル | ライセンス | アクション |
---|---|---|
110008014695.pdf (238.7 kB)
|
|
Item type | 会議発表論文 / Conference Paper(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2012-03-28 | |||||
タイトル | ||||||
言語 | ja | |||||
タイトル | 1-2 コンクリートの表層特性に関する実験研究(材料・構造系) | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | 1-2 Experimental study on property of concrete surface | |||||
言語 | ||||||
言語 | jpn | |||||
キーワード | ||||||
主題 | コンクリート表層 | |||||
キーワード | ||||||
主題 | 吸水性 | |||||
キーワード | ||||||
主題 | コンクリートの単位水量 | |||||
キーワード | ||||||
主題 | concrete surface | |||||
キーワード | ||||||
主題 | water absorption | |||||
キーワード | ||||||
主題 | water content per unit volume of concrete | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_5794 | |||||
資源タイプ | conference paper | |||||
著者 |
佐藤, 茂治
× 佐藤, 茂治× 地濃, 茂雄 |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | コンクリートの表層面は意匠上かつ耐久性状上、重要な部位であることに着目し、その劣化現象を解明する上での基礎的実験を行った。その結果、水セメント比が等しく同一強度のコンクリートでも、単位水量(スランプ)が相違すれば、セメントペースト量や骨材量も異なることになり、表層モルタルの吸水性状が相違することを実験的に明らかにし、これより耐久性に及ぼす表層特性を考察した。 | |||||
書誌情報 |
日本建築学会北陸支部研究報告集 巻 53, p. 1-2, 発行日 2010-07 |
|||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0385-9622 | |||||
書誌レコードID | ||||||
収録物識別子タイプ | NCID | |||||
収録物識別子 | AN00188761 | |||||
権利 | ||||||
権利情報 | 社団法人日本建築学会 | |||||
権利 | ||||||
権利情報 | 本文データは学協会の許諾に基づきCiNiiから複製したものである | |||||
著者版フラグ | ||||||
出版タイプ | VoR | |||||
出版タイプResource | http://purl.org/coar/version/c_970fb48d4fbd8a85 | |||||
出版者 | ||||||
出版者 | 日本建築学会 | |||||
関係URI | ||||||
関連名称 | http://ci.nii.ac.jp/naid/110008014695 |